See how 316L stainless and Hastelloy C276 compare in concentrated hydrochloric acid. Stainless steel 316L is good in corrosive environments but halogens corrode it quickly due to the complexation in the passivation layer.

You could see the black layer just after 30 minutes in acid. Nickel-based Hastelloy C 276 is much more stable – not a trace of damage. Hastelloy C-276 SABRe Systems are now available. What does this mean for you? Superior chemical compatibility, opening up a wider scope of chemistries in continuous flow! Have a particularly corrosive or halide dependent process you want to carry out in flow?

Contact us to discuss feasibility and arrange a trial. https://stolichem.com/products/

Would you benefit from the flow?

Best in class mixing performance.

See our product range and the SABRe – the reactor that can do most batch processes in flow with exceptional heat and mass transfer and lightning-fast mixing.

Other news:

CHEMUK 2021 exhibition

CHEMUK 2021 exhibition

Visit us and see our new Scalable Agitated Baffle Reactor (SABRe) at CHEMUK2021, NEC Birmingham, stand B25 September 15th-16th

ChemUK 2023

ChemUK 2023

Let’s meet at ChemUK 2023, stand H76. Free to visit. 10-11 May 2023.

Achema 2022

Achema 2022

Visit us at stand F62 in Achema 2022, 22-26 August, Frankfurt

Plug flow (tubular) reactor

Plug flow (tubular) reactor

Tubular reactors (incorrectly, “plug flow”) – the simplest continuous reactors. See Daniel Lambden’s overview of the tubular reactors.